PDF Determining Specific Grinding Rate of Coarse McGill University
the + 105 µm material in the ball mill; that is, the fraction of total mill power that is usefully used to size reduce coarse material (+ 105 µm) to material finer than 105 µm. ... The fact that they differ at the coarser sizes may be because the retention time may be higher for the coarser sizes and thus in the H/F method the τ should be ...