Microstructure and properties of CuCrSiC insitu composite coatings ...
The oxide and grease on the substrate surface are removed with 600 mesh sandpaper. After sandblasting, the substrate was ultrasonically cleaned in an alcohol solution for 5 min and then dried. ... it was weighed out according to the ratio in Table 1 and put into a planetary ball mill with a 4:1 ball to powder ratio. It was then processed at 150 ...