Characterization and calcination behavior of a lowgrade manganese ore ...
A 120gram piece of the ore sample ( mm) and a 20gram piece of the ore sample powder (< 74 microns) were each calcined in an argon flow rate of 1 N L/min in a tube furnace. The heating rate was adjusted on 10 °C/min (10 K/min) and the calcination tests were continued for 60 min at 900 °C (1173 K), as observed in A similar ...